This document describes the shot peening process, including shot peening media, equipment, and operating procedures.
This GE standard operating manual covers shot peening for engine work, identified as SPM 70-47-01, dated 04/01/2011. It explains the shot peening process, including the use of metal, glass, and ceramic media to create residual compressive stress on part surfaces and improve resistance to stress corrosion and cyclic fatigue.
The document describes general, manual, automatic, and computer-controlled shot peening equipment, along with Almen test coupon fixtures and media requirements. It includes safety warnings about protective equipment, dust hazards from materials such as nickel and titanium, static charge, arc damage inspection, and grinding and pickling steps referenced to other tasks. This manual is written in Chinese.
| Direct impact angle | 35 degrees |
|---|---|
| Almen coupon contour tolerance | 0.060 inch (1.5 mm) |
| Maximum nozzle wear | 15% of nominal diameter |
| Maximum air jet wear | 10% of nominal diameter |
| Cast steel shot hardness | 55-62 HRC |
| Cast steel shot specification | AMS 2431/2 |
Shot peening uses metal, glass, or ceramic media to form residual compressive stress on the part surface, improving resistance to stress corrosion and cyclic fatigue.
No. Manual shot peening is not allowed for these parts unless the process document specifically states it and authorizes a specific location on the workpiece.
Visually inspect the probe-to-workpiece contact area for melting or pits, then repair the affected area by grinding and pickling before inspection and re-peening.
All shot must pass through the screening device before reuse to remove broken, oversize, and undersize particles.