The Toray TAC VG5 waterless CTP plate user manual provides safety guidelines, required conditions, processing steps, and chemical handling instructions.
This manual explains how to use Toray TAC VG5 waterless CTP plates, including safety precautions, the conditions required for waterless CTP printing, and how the plate differs from traditional wet plate-making and printing methods. It covers plate-making steps such as exposure, development, plate inspection, and troubleshooting, followed by printing preparation and printing procedures.
The manual also provides instructions for processing solutions used with automatic developing machines: CP-Y pre-treatment solution, PA-F post-treatment solution, defoaming agent S, and post-treatment auxiliary agent AC-2, including their uses, handling, storage, and disposal. This manual is written in Chinese.
| Plate type | Thermal negative photosensitive TAC plate |
|---|---|
| Revision | 1 |
| Storage temperature | Room temperature 25 °C or below |
| Storage humidity | 70% or below |
| CP-Y pre-treatment solution composition | Ethylene glycol derivative 85%, organic alkali 15% |
| PA-F post-treatment solution composition | Ethylene glycol derivative 10%, fuel/surfactant 3%, water 87% |
| Defoaming agent S dosage | 100 mL per 20 L of post-treatment tank solution |
| AC-2 auxiliary agent dosage | 50 mL per 20 L of post-treatment tank solution |
Managers must train operators on safety before plate-making work. Operators should read the automatic developing machine safety notes and the MSDS for the processing solutions, wear protective gloves, wash after work, and ensure adequate ventilation in the developing room.
Store the plates in a cool place away from high temperature, high humidity, and direct sunlight, at room temperature of 25 °C or below and humidity of 70% or below. Handle them so the surface film is not scratched or peeled.
Add CP-Y to the pre-treatment tank with a hand pump. It normally only needs periodic top-up for amounts lost through plate contact, and full replacement is recommended once a year. Water contamination greatly reduces positive plate development performance.
PA-F stains the silicone layer stripped during development to improve plate inspection. AC-2 neutralizes pre-treatment solution that has entered the post-treatment solution and improves its staining performance.