AZ P4000 Series Positive Tone Photoresists Datasheet

Technical datasheet for AZ P4000 Series positive tone photoresists, detailing film thickness grades, processing steps, optical constants, and dielectric…


AZ P4000 Series Positive Tone Photoresists Datasheet - cover page
Brand
AZ
Category
Other Electronics
Document type
Datasheet
Language
English
Pages
7
File format
PDF
File size
771 KB
Published
15 October, 2026
Updated
15 October, 2026
MD5 checksum
AE6E4F79616BCCE3CAFC0533E851DF7C

About this manual

This document is a technical datasheet for the AZ P4000 Series of positive tone photoresists. These materials are engineered with a special Photo Active Compound (PAC) to prevent plating solution poisoning and extend bath life, while offering excellent substrate adhesion for wet etch applications. The series is compatible with a wide range of electroplating solutions and features safe solvent properties.

What's inside

  • General purpose positive tone photoresists
  • Thickness Grades
  • Typical Process
  • Optical Constants
  • Typical Spin Curves
  • Au Plating Results
  • Dielectric Insulator Properties
  • Fluid Viscosities
  • Dill Modelling Parameters
  • Process Considerations

Specifications

Film Thickness Range (AZ P4110)1.0 – 3.0µm
Film Thickness Range (AZ P4620)6.0 - >20µm
Film Thickness Range (AZ P4903)10.0 - >30µm
Soft Bake Temperature90 -115C
Exposure Wavelength Sensitivity310 and 450nm
Recommended Exposure Wavelength365 -436nm
Dielectric Constant @ 200º C4.02
Breakdown Voltage @ 250º C674 V/µm
Viscosity (AZ P4620)536 cSt

Frequently asked questions

What is the special feature of the PAC in AZ P4000?

The special PAC is engineered to prevent poisoning of plating solutions and extend plating bath life.

Can AZ P4000 be used as a dielectric insulator?

Yes, the photoresists may be thermally cured after develop to form stable dielectric isolators.

What developer types are recommended for AZ P4000?

Inorganic (IN) developers are recommended, with AZ 400K series specifically suggested for this series.

Is a rehydration step required for thick films?

Yes, films thicker than 4.0µm require a rehydration hold between soft bake and exposure.