Nippon Paint Hi-Pon 20-07 Epoxy Zinc Phosphate 70 Technical Data Sheet

Nippon Paint Hi-Pon 20-07 Epoxy Zinc Phosphate 70 technical data sheet: two-pack zinc phosphate epoxy coating properties, surface prep and application.


Nippon Paint Hi-Pon 20-07 Epoxy Zinc Phosphate 70 Technical Data Sheet - cover page
Brand
Nippon Paint
Category
Chemical products
Document type
Datasheet
Language
English
Pages
4
File format
PDF
File size
200 KB
Published
17 November, 2026
Updated
17 November, 2026
MD5 checksum
233A68D99A5D620FAD7E992797DA9317

About this manual

Hi-Pon 20-07 Epoxy Zinc Phosphate 70 is a two-pack, high build, fast drying zinc phosphate epoxy coating from Nippon Paint, described as a universal anti-corrosive for all areas according to ISO 12944. It is an anti-corrosive primer and/or intermediate coating for corrosion protection of steel and other substrates in atmospheric exposure, supplied in Buff and Red with a low sheen finish.

The technical data sheet covers general properties (72 ± 2 % volume solids, 1.46 - 1.56 kg/l specific gravity when mixed, 260 g/L VOC, 100 - 250 µm dry film thickness), surface preparation to Sa 2½, the 4:1 base to hardener mixing ratio, conditions during application, airless spray details, drying and recoating times, recommended intermediate and topcoats, packaging, storage and safety precautions.

What's inside

  • Product Description
  • Intended Use
  • General Properties
  • Surface Preparation
  • Application Guide
  • Application Method
  • Recommended Painting System
  • Packaging
  • Storage
  • Safety Precaution

Specifications

ColourBuff & Red
Gloss LevelLow sheen
Volume Solids72 ± 2 %
Specific Gravity1.46 - 1.56 kg/l (mixed)
Flash PointBase 33°C, Hardener 35°C, Mix 33°C
VOC260 g/L (mix, by calculation)
Typical Thickness100 - 250 µm dry film; 140 - 360 µm wet film
Theoretical Coverage7.2 m2/litre at 100 µm DFT; 2.9 m2/litre at 250 µm DFT
Mixing RatioBase : hardener = 4:1 by volume
Shelf LifePart A: 12 months (25°C); Part B: 12 months (25°C)

Frequently asked questions

How should bare steel be prepared before applying Hi-Pon 20-07?

Bare steel should be prepared with abrasive blast cleaning to Sa 2½ (ISO 8501-1:2007) to achieve a surface profile of 50 - 70 µm.

What is the mixing ratio of Hi-Pon 20-07?

The base and hardener are mixed at 4:1 by volume, thoroughly, before use, with an induction time of 15 minutes.

What application conditions should be avoided?

Avoid application when the temperature is below 10°C or relative humidity exceeds 85%, and keep the steel surface temperature at least 3°C above the dew point.

What is the recommended application method?

Airless spray gives the best result; brush and roll are suitable for stripe coating and very small areas.