This manual describes the Liming WM0012-6 PU-RIM combination material used for reaction injection molding of glass window edging, including chemical…
The document provides a product manual for the Liming WM0012-6 PU-RIM combination material. It consists of two components: Component A (combination polyether) and Component B (modified isocyanate). The material is designed for reaction injection molding processes to produce polyurethane glass overall window edging materials. This manual is written in Chinese.
| Component A Viscosity (25°C) | 1800±400 mPa·s |
|---|---|
| Component A Density (20°C) | 1.03±0.05 g/cm³ |
| Hardness (Shore A) | 90±4 |
| Tensile Strength | ≥12 MPa |
| Elongation at Break | ≥200 % |
| Tear Strength | ≥35 N/mm |
The material ratio is 100 parts of Component A to 60±4 parts of Component B.
Before use, the entire bucket of raw material should be placed on a rotating mixer and rotated for 1 hour.
The material should be stored in a sealed container at temperatures between -5°C and 35°C.