DELO DUALBOND light/heat curing acrylic adhesive instructions for surface preparation, application, light and heat curing, storage, and safety.
This document provides instructions for DELO DUALBOND light/heat curing acrylic adhesive. It applies to bonding, coating, fixing, and sealing processes in electronics, electrical engineering, microelectronics, optics, and precision engineering.
It covers substrate cleaning and preparation, adhesive preparation and temperature conditioning, dispensing and processing, light and heat curing requirements, storage conditions, and UV skin and eye protection. Contact DELO for any questions. This manual is written in Chinese.
| Light wavelength range | 315 nm to 450 nm |
|---|---|
| UVA curing wavelength range | 315 to 420 nm |
| VIS curing wavelength range | 380 to 450 nm |
| Maximum cured adhesive thickness | 2 to 4 mm |
| Processing temperature | +18 °C to +25 °C |
The light wavelength range must be between 315 nm and 450 nm.
Process the product at +18 °C to +25 °C with 20 % to 70 % relative humidity.
Yes, the adhesive can be heat cured or light cured, and shadow areas can be fully cured by subsequent heating.