Alpha Assembly Solutions SMT Troubleshooting Guide

This document is a troubleshooting guide for common SMT assembly issues.


Alpha Assembly Solutions SMT Troubleshooting Guide - cover page
Brand
Alpha Assembly Solutions
Category
Other
Document type
Other
Language
English
Pages
24
File format
PDF
File size
3 MB
Published
03 November, 2023
Updated
03 November, 2023
MD5 checksum
522F4D73E296C2EA6BF332A8BB667514

About this manual

This guide from Alpha Assembly Solutions provides troubleshooting advice for common SMT assembly issues by process defect. Its table of contents covers defects such as bridging, non-wet open, insufficient fill, insufficient solder, random solder balls, tombstoning, voiding, BGA head-on-pillow, and grainy joints.

Each section describes possible causes and recommendations related to areas such as PCB, stencil, screen printer, component placement, reflow profile, and solder paste. The guide advises contacting an Alpha representative if an issue is not resolved after following the steps.

What's inside

  • Bridging
  • Non-Wet Open
  • Insufficient Fill
  • Insufficient Solder
  • Random Solder Balls
  • Tombstoning
  • Voiding
  • BGA Head-on-Pillow
  • Grainy Joints

Frequently asked questions

What is bridging in SMT assembly?

Bridging is solder connecting, in most cases misconnecting, two or more adjacent pads that come into contact to form a conductive path.

What is a non-wet open?

A non-wet open, also called non-wet or lifted ball, occurs when the solder sphere and solder paste on the BGA have no physical contact with the pad after reflow.

What is a grainy joint?

A grainy joint, sometimes called 'Cold Solder,' is recognized by dark, non-reflective, rough surfaces from an alloy that is normally bright and shiny.

What cooling rate is recommended for grainy joints?

The guide recommends ensuring the alloy cooling rate from molten solder is 3-8°C/sec.