This file is about the troubleshooting of LUXAPOOL Epoxy paint film defects
LUXAPOOL Epoxy is a pool coating, and this guide explains common film defects that can occur during or after application. It covers causes and remedies for issues such as blooming, foreign matter, staining, bubbling, blistering, delamination, and chalking.
The guide also outlines pool water chemistry maintenance, including waiting periods before filling, chemical addition methods, and target ranges for total alkalinity, pH, calcium hardness, and chlorine.
| Total alkalinity | 160-180 ppm (adjust close to 180 ppm) |
|---|---|
| pH | 7.4-7.8 (adjust close to 7.6) |
| Calcium hardness | 280-320 ppm |
| Chlorine | Under 3 ppm, ideally 1-2 ppm |
| Fill delay after painting | At least 10 days in summer or 14 days in winter |
| Full cure before scraping foreign matter | 5 days |
The entire coat of paint should be removed and a new coat applied.
At least 10 days in summer or 14 days in winter.
Adjust close to 180 ppm and maintain within 160-180 ppm.
Allow the epoxy to set tack free, then lightly sand with very fine wet and dry sandpaper and remove residue with a vacuum cleaner.