YTL-VR is a high-performance, cold-applied, non-tread self-adhesive waterproof roll material made of a special rubber asphalt self-adhesive layer, an imported anti-skid strong cross-laminated membrane as the surface material, and a non-stick separation paper/membrane as the bottom separation layer. When the bottom separation paper/membrane is removed, the roll can be firmly adhered to the base and has the characteristics of high tear resistance and good dimensional stability.
This is the Chinese product manual (产品说明书) for 易贴灵 YTL-VR, a cold-applied, self-adhesive waterproofing underlayment for pitched roofs made by GCP Applied Technologies. The membrane is built from a rubber-asphalt self-adhesive layer, an imported slip-resistant cross-laminated film surface and a release paper or film backing; the sheet is simply pressed onto the prepared substrate after the release liner is removed.
The document lists the applications (pitched roofs, old roof repair, sealing around door and window frames, exterior wall moisture and vapor protection) and the advantages of the sheet, then gives physical properties to JC/T 1068-2008, surface preparation and primer instructions, laying, lapping and repair procedures, wet and dry laying methods, precautions and limitations, roll sizes and storage, quality assurance and GCP technical service contacts. This manual is written in Chinese.
| Standard | JC/T 1068-2008 |
|---|---|
| Thickness | 1.0 mm or 1.5 mm |
| Roll length | 30 m/roll or 20 m/roll |
| Tensile force | ≥ 70 N/25 mm |
| Elongation at break | ≥ 200 % |
| Nail shank tear strength | ≥ 40 N |
| Peel strength, underlayment to underlayment | ≥ 1.2 N/mm |
| Peel strength, underlayment to aluminum sheet | ≥ 1.5 N/mm |
| Nail shank watertightness | No water seepage |
Laying should be done when the ambient, roof and membrane temperatures are not below 5 ºC (40 ºF) or in better weather; the roof covering must be installed under the same conditions.
Both the long and short edge laps must be at least 80 mm wide and rolled firmly with the matching roller.
It must not be exposed to sunlight for long periods; covering within 14 days is recommended.
Clean the damaged spot and patch it directly with 易贴灵 YTL-VR, extending at least 100 mm beyond the damage.