Concrete Preservation Technologies Ltd PatchGuard Anode Spacing Specification

This is about steel density ratio, the table provides the maximum spacing (mm) of different types of steel density ratios.


Concrete Preservation Technologies Ltd PatchGuard Anode Spacing Specification - cover page
Brand
Concrete Preservation Technologies Ltd
Document type
Product Leaflet
Language
English
Pages
1
File format
PDF
File size
86 KB
Published
26 October, 2023
Updated
26 October, 2023
MD5 checksum
BCF70EC799056E47B6FCBA1C22216C21

About this manual

This document provides spacing guidelines for PatchGuard galvanic anodes in concrete, categorized by corrosion environment. Spacing varies with steel density ratio and chloride content, with tables for low and high corrosion conditions. It also notes compatibility with high-quality repair mortar and no restriction on resistivity values.

What's inside

  • Maximum Spacing
  • Steel Density Ratio
  • Chloride Content
  • Corrosion Environment
  • PatchGuard Anodes

Specifications

Maximum Spacing for Steel Density Ratio 0.3600 mm
Maximum Spacing for Chloride Content >1.9%Reduced spacing required

Frequently asked questions

What is the maximum spacing for steel density ratio 0.3?

600 mm.

What should be done if chloride content exceeds 1.9%?

Anode spacing will need to be reduced.

Download PDF (86 KB)