Kurt J. Lesker Company KJL-6000 Series Thermocouple Vacuum Gauge Tube Operator's Manual

KJL-6000 series thermocouple vacuum gauge tube operator's manual, including the product specifications, accuracy, response time, baking temperature, positive pressure rating, mounting orientation, standard tube materials, troubleshooting procedure, troubleshooting notes, etc.


Kurt J. Lesker Company KJL-6000 Series Thermocouple Vacuum Gauge Tube Operator's Manual - cover page
Brand
Kurt J. Lesker Company
Category
Other Electronics
Document type
User Manual
Language
English
Pages
4
File format
PDF
File size
363 KB
Published
19 October, 2023
Updated
19 October, 2023
MD5 checksum
9C1285207E3DCD14281C06B26F477284

About this manual

This document serves as the operator's manual for the KJL-6000 series thermocouple vacuum gauge tube manufactured by the Kurt J. Lesker Company. It details the device's specifications, including a pressure range from 1 x 10-3 to 1 Torr, and describes the operating principles based on heat transfer from a heated filament to gas molecules. The manual also outlines the standard materials used, such as stainless steel for the cup and stem, and nickel-plated Kovar for connector pins.

What's inside

  • Specifications
  • Troubleshooting Procedure
  • Operating Principles
  • Mounting Orientation
  • Troubleshooting Notes
  • Operating Principles
  • Calibration and Stabilization
  • Safety Warnings

Specifications

Pressure Range1 x 10-3 to 1 Torr
Accuracy± 1 mTorr from 1 to 20 mTorr
Response Time< 1 second for 1 mTorr up to atmosphere
Bakeout Temperature100 °C (212 °F)
Positive Pressure RatingTested to 1200 PSIG for operation up to 300 PSIG
Standard Tube MaterialsStainless steel (cup, stem and flange)

Frequently asked questions

How do I verify if a KJL-6000 thermocouple tube is functional?

Use the ohmmeter setting on a multimeter to measure the resistance between pins 3 and 5. A reading of 19 ohms +/- 2 ohms indicates the tube is good.

What is the recommended mounting orientation for the tube?

Ideally, the open end should point down so as to be self-draining should any vapors condense.

How long should the tube outgas before use?

It is a good idea to allow the tube to outgas in the vacuum system for approximately 24 hours, but allow at least 15 minutes for the tube to stabilize.

Can thermocouple gauges be used to monitor backfilling of loadlocks?

No, thermocouple gauges should definitely not be used to monitor the backfilling of loadlocks as it is possible to create a dangerous overpressure situation.

Download PDF (363 KB)